Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® T110 PRO - Copolyester - SK Chemicals

Material Data Center offers the following functions for ECOZEN® T110 PRO:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
ECOZEN® is a glycol-modified polyethylene terephthalate with exceptional transparency and chemical resistance.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.0035 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 47 MPa ISO 527
Yield strain 6.5 % ISO 527
Stress at break 48 MPa ISO 527
Strain at break 238 % ISO 527
Flexural modulus, 23°C 1670 MPa ISO 178
Flexural strength 66 MPa ISO 178
Izod notched impact strength, +23°C 93 kJ/m² ISO 180/1A
ASTM Data
Tensile Strength at Yield 48 MPa ASTM D 638
Tensile Strength at Break 54 MPa ASTM D 638
Elongation at Yield 6.6 % ASTM D 638
Elongation at Break 285 % ASTM D 638
Flexural Modulus 1658 MPa ASTM D 790
Flexural Strength 70.6 MPa ASTM D 790
Rockwell Hardness R 115 - ASTM D 785
Izod Impact notched, 1/8 in 860 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 82 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 97 °C ISO 75-1/-2
ASTM Data
DTUL @ 66 psi 99 °C ASTM D 648
DTUL @ 264 psi 85 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 84 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1230 kg/m³ ASTM D 792
Characteristics
Special Characteristics
Heat stabilized or stable to heat, Transparent
Features
Copolymer
Chemical Resistance
General Chemical Resistance
Certifications
Contains renewable resources, Food contact, RoHS compliant
Applications
Packaging
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.