Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1185 A - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1185 A:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
DESCRIPTION
Elastollan 1185 A is a polyether based TPU

SPECIAL PROPERTIES
excellent resistance to hydrolysis and good flexibility at low temperature,
resistance to microbiological attack, good wear performance,
high tensile strength, good damping behavior

TYPICAL APPLICATIONS
cable sheathing, plugs and terminations, hoses, films,
damping elements

OTHER HINTS
predrying: 2-3h at 100-110°C (air circulating oven)
or 80-90°C (dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties
MFR range: in various MFR ranges provided

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 20 MPa ISO 527
Stress at 50% strain 5 MPa ISO 527
Strain at break >50 % ISO 527
Charpy notched impact strength, +23°C N kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C N kJ/m² ISO 179/1eA
Tensile notched impact strength, +23°C 580 kJ/m² ISO 8256/1
Stress at 100% elongation 6 MPa ISO 527
Stress at 300% elongation 10 MPa ISO 527
Stress at break TPE 45 MPa ISO 527
Strain at break TPE >300 % ISO 527
Compression set at 23 °C, 24h 25 % ISO 815
Compression set at 70 °C, 24h 45 % ISO 815
Tear strength 70 kN/m ISO 34-1
Abrasion resistance 25 mm³ ISO 4649
Shore A hardness 87 - ISO 7619-1
Shore D hardness 36 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min -42 °C ISO 11357-1/-2
Burning Behav. at thickness h HB class IEC 60695-11-10
Yellow Card available yes - -
Oxygen index 23 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Dissipation factor, 100Hz 300 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 950 E-4 IEC 62631-2-1
Volume resistivity 1E10 Ohm*m IEC 62631-3-1
Surface resistivity 1E15 Ohm IEC 62631-3-2
Electric strength 35 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1120 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 210 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Diagrams
Viscosity-shear rate , Elastollan® 1185 A, (TPU-ARET), BASF PU
Shearstress-shear rate , Elastollan® 1185 A, (TPU-ARET), BASF PU
Dynamic Shear modulus-temperature , Elastollan® 1185 A, (TPU-ARET), BASF PU
Stress-strain , Elastollan® 1185 A, (TPU-ARET), BASF PU
Secant modulus-strain , Elastollan® 1185 A, (TPU-ARET), BASF PU
Stress-Strain (TPE) , Elastollan® 1185 A, (TPU-ARET), BASF PU
Stress-strain (isochronous) 23°C, Elastollan® 1185 A, (TPU-ARET), BASF PU
Creep modulus-time 23°C, Elastollan® 1185 A, (TPU-ARET), BASF PU
Creep curve 23°C, Elastollan® 1185 A, (TPU-ARET), BASF PU
Characteristics
Processing
Injection Molding, Profile Extrusion, Blow Molding
Delivery form
Pellets
Regional Availability
Other text information
Injection molding
Barrel temperature : 195 - 210 °C
Melt temperature : 210 °C
Mold temperature: 25 - 40 °C
Profile extrusion
Barrel temperature : 160 - 190 °C
Blow molding
Barrel temperature : 160 - 195 °C
Mold temperature : 40 - 80 °C
Application examples
Handrail with Modular Design
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com