Any use of this information falls under the rules of our
disclaimer.
Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt volume-flow rate, MVR |
8[1] |
cm³/10min |
ISO 1133 |
Temperature |
235 |
°C |
- |
Load |
5 |
kg |
- |
1: | Data based on raw material |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Modulus |
1440[2] |
MPa |
ISO 527 |
Yield stress |
43[2] |
MPa |
ISO 527 |
Charpy notched impact strength, +23°C |
11[2] |
kJ/m² |
ISO 179/1eA |
2: | Data based on raw material |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Melting temperature, 10°C/min |
180[3] |
°C |
ISO 11357-1/-3 |
3: | Data based on raw material |
Other properties | Value | Unit | Test Standard |
Density |
1010[4] |
kg/m³ |
ISO 1183 |
4: | Data based on raw material |
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament, Natural Color
Special Characteristics
High impact or impact modified
Features
Good Adhesion, Low Odor
Chemical Resistance
General Chemical Resistance
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com