Processing/Physical Characteristics | Value | Unit | Test Standard |
Other Standards[S] |
Molding shrinkage, parallel |
0.2 |
% |
BS-2782 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
Other Standards[S] |
Tensile Strength |
69 |
MPa |
BS-2782 |
Flexural strength |
157 |
MPa |
BS-2782 |
Compressive Strength |
196 |
MPa |
BS-2782 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
ASTM Data |
UL 94 Flame rating |
V-0 |
- |
UL 94 |
Electrical properties | Value | Unit | Test Standard |
ASTM Data |
Arc Resistance |
185 |
s |
ASTM D 495 |
Other Standards[S] |
Surface resistivity |
1E9 |
Ohm |
DIN 53482 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Other Standards[S] |
Water absorption |
0.3 |
% |
BS-2782 |
Density |
1700 |
kg/mĀ³ |
BS-2782 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Characteristics
Processing
Compression Molding
Delivery form
Sheet Molding Compound
Special Characteristics
Anti-static
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com