Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FORTRON® ICE 504L - PPS-GF40 - Celanese

Material Data Center offers the following functions for FORTRON® ICE 504L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Fortron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

FORTRON ICE 504L is a 40% glass fiber reinforced polyphenylene sulfide, that belongs to our new generation of Fortron® PPS.
This new technology allows optimization of molding conditions with faster cycle times. Due to the faster crystallization of the material at a higher temperature, the option of mold wall temperature reduction can be subject of advanced process optimization. The potential for optimization of Fortron® ICE by cycle time reduction is possible by standard cavity surface temperatures of 140°C. The potential for lowering the mold temperature must be checked individually and it depends on process and part design.
 



Flammability @1.6mm nom. thickn.V-0-
Flammability at thickness h (0.38 mm)V-0-
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.3 % ISO 294-4, 2577
Molding shrinkage, normal 0.6 % ISO 294-4, 2577
Spec. heat capacity of melt 1500 J/(kg K) -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 15100 MPa ISO 527
Stress at break 202 MPa ISO 527
Strain at break 1.9 % ISO 527
Charpy impact strength, +23°C 53 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 53 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 10 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 280 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 90 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 270 °C ISO 75-1/-2
Temp. of deflection under load, 8.00 MPa 215 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 26 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 42 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 0.4 mm -
Oxygen index 47 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 4.1 - IEC 62631-2-1
Dissipation factor, 1MHz 20 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Other propertiesValueUnitTest Standard
Water absorption 0.02 % Sim. to ISO 62
Density 1650 kg/m³ ISO 1183
Diagrams
Stress-strain , FORTRON® ICE 504L, PPS-GF40, Celanese
Secant modulus-strain , FORTRON® ICE 504L, PPS-GF40, Celanese
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Certifications
Drinking water contact
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.