Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ G1301A-M61 - PA9T-I-GF30 - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ G1301A-M61:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts


Genestar G1301A-M61 Black is toughened 30%GF reinforced injection moulding grade.


The main features are:

  • Performance at high temperatures
  • Low water absorption and retention of its initial properties
  • Ductility and impact strength

This grade is suitable for:
  • Quick connector
  • Structural parts in harsh chemical and thermal environments that require a certain ductility.



Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.3 % ISO 294-4, 2577
Molding shrinkage, normal 0.9 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 8980 MPa ISO 527
Stress at break 175 MPa ISO 527
Strain at break 3 % ISO 527
Charpy notched impact strength, +23°C 17 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 300 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 125 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 270 °C ISO 75-1/-2
ASTM Data
Coefficient of Thermal Expansion, MD 20 E-6/K ASTM D 696
Coefficient of Thermal Expansion, TD 46 E-6/K ASTM D 696
Other propertiesValueUnitTest Standard
Water absorption 0.19 % Sim. to ISO 62
Density 1340 kg/m³ ISO 1183
Diagrams
Stress-strain , Genestar™ G1301A-M61, PA9T-I-GF30, Kuraray
Secant modulus-strain , Genestar™ G1301A-M61, PA9T-I-GF30, Kuraray
Specific volume-temperature (pvT) , Genestar™ G1301A-M61, PA9T-I-GF30, Kuraray
Characteristics
Processing
Injection Molding
Delivery form
Black
Additives
Lubricants, Release agent
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Features
Barrier Properties, Creep Resistance, Fatigue Resistance, High Crystallinity, Thermal Stability, Tribologic Grade, Weldable
Chemical Resistance
Acid Resistance, Alkali Resistance, General Chemical Resistance, Environmental Stress Crack Resistance, Solvent Resistance, Grease Resistance, Hydrolytically Stable, Oil Resistance
Applications
Automotive, General Purpose
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.