Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HOSTAFORM® C 13021 XAP® - POM - Celanese

Material Data Center offers the following functions for HOSTAFORM® C 13021 XAP®:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Hostaform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
POM copolymer Easy flowing Injection molding type for precision molded parts and thin-walled molded parts with high rigidity, hardness and toughness; good chemical resistance to solvents, fuel and strong alkalis as well as good hydrolysis resistance; high resistance to thermal and oxidative degradation. Emission according to VDA 275 < 10 mg/kg Monomers and additives are listed in EU-Regulation (EU) 10/2011 FDA compliant according to 21 CFR 177.2470 Burning rate ISO 3795 and FMVSS 302 < 75 mm/min for a thickness more than 1 mm. Ranges of applications: automotive engineering, precision engineering, electric and electronical industry, domestic appliances. FDA = Food and Drug Administration (USA) FMVSS = Federal Motor Vehicle Safety Standard (USA)

Flammability @1.6mm nom. thickn.HB-
Flammability at thickness h (3 mm)HBUL recognition (h)
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 12 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Molding shrinkage, parallel 2.0 % ISO 294-4, 2577
Molding shrinkage, normal 1.8 % ISO 294-4, 2577
Density of melt 1200 kg/m³ -
Thermal conductivity of melt 0.155 W/(m K) -
Spec. heat capacity of melt 2210 J/(kg K) -
Ejection temperature 140 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2900 MPa ISO 527
Yield stress 65 MPa ISO 527
Yield strain 9 % ISO 527
Nominal strain at break 25 % ISO 527
Charpy impact strength, +23°C 200 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 200 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6.5 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 6 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 166 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 106 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 110 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.0 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4 - IEC 62631-2-1
Relative permittivity, 1MHz 4 - IEC 62631-2-1
Dissipation factor, 100Hz 20 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 50 E-4 IEC 62631-2-1
Volume resistivity 1E12 Ohm*m IEC 62631-3-1
Surface resistivity 1E14 Ohm IEC 62631-3-2
Electric strength 35 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 0.65 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1410 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 - 120 °C -
Pre-drying - Time 3 - 6 h -
Processing humidity ≤0.1 % -
Melt temperature 180 - 190 °C -
Mold temperature 60 - 120 °C -
Diagrams
Viscosity-shear rate , HOSTAFORM® C 13021 XAP®, POM, Celanese
Shearstress-shear rate , HOSTAFORM® C 13021 XAP®, POM, Celanese
Stress-strain , HOSTAFORM® C 13021 XAP®, POM, Celanese
Secant modulus-strain , HOSTAFORM® C 13021 XAP®, POM, Celanese
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Features
Low Emission, Thermal Stability, Copolymer
Chemical Resistance
Alkali Resistance, Solvent Resistance, Hydrolytically Stable, Oxidation Resistance
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR
Applications
Automotive, Electrical and Electronical
Other text information
Injection molding
To achive low emission values pre drying using a recirculating air dryer (100 to 120 °C / max. 40 mm layer / 3 to 6 hours) is recommended.

Max. Water content 0,1 %
Standard injection moulding machines with three phase (15 to 25 D)
plasticating screws will fit.

Conditioning e.g. moisturizing is not necessary.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.