Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Hylon® N1000STL HF - PA66 - Ravago Manufacturing Americas

Material Data Center offers the following functions for Hylon® N1000STL HF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Hylon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 1.9 / * % ISO 294-4, 2577
ASTM Data
Mold Shrinkage, MD 0.019 mm/mm ASTM D 955
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Yield stress 57 / - MPa ISO 527
Strain at break 45 / - % ISO 527
Flexural modulus, 23°C 1900 / - MPa ISO 178
Izod notched impact strength, +23°C 60 / - kJ/m² ISO 180/1A
ASTM Data
Tensile Strength at Yield 57.9 / - MPa ASTM D 638
Elongation at Break 50 / - % ASTM D 638
Flexural Modulus 1830 / - MPa ASTM D 790
Flexural Strength 70.3 / - MPa ASTM D 790
Izod Impact notched, 1/8 in 850 / - J/m ASTM D 256
Thermal propertiesdry / condUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 64 / * °C ISO 75-1/-2
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 0.787 mm -
DTUL @ 264 psi 62 °C ASTM D 648
Other propertiesdry / condUnitTest Standard
Density 1080 / - kg/m³ ISO 1183
Density 1080 kg/m³ ASTM D 792
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Lubricants
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.