KURARITY is non-crystalline block copolymer and does not have melting point.
All the KURARITY grades show similar low temperature properties which result from Tg of
poly (n-butyl acrylate) or poly (n-butyl acrylate/2-ethylhexyl acrylate) and heat resistance
from Tg of PMMA.
LA series : n-butyl acrylate based block copolymers.
Suitable Applications: For Molding, Compound, Additives.
Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt flow index, MFI |
1.5 |
g/10min |
ISO 1133 |
Temperature |
190 |
°C |
- |
Load |
2.16 |
kg |
- |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Strength |
17 |
MPa |
ISO 527 |
Flexural modulus, 23°C |
750 |
MPa |
ISO 178 |
Charpy notched impact strength, +23°C |
30 |
kJ/m² |
ISO 179/1eA |
Tensile Strength |
25 |
MPa |
ISO 37 |
Shore A hardness |
90 |
- |
ISO 7619-1 |
Shore D hardness |
47 |
- |
ISO 7619-1 |
Other Standards[S] |
Stress at 100% elongation |
19 |
MPa |
ISO 37 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
Other Standards[S] |
Thermal Conductivity, solid state |
0.17 |
W/(m K) |
ASTM E 1530 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Electrical properties | Value | Unit | Test Standard |
Other Standards[S] |
Dissipation Factor, 60 Hz |
0.0394 |
- |
JIS C 2138 |
Dissipation Factor, 1 MHz |
0.0448 |
- |
JIS C 2138 |
Dielectric Constant, 60 Hz |
4.56 |
- |
JIS C 2138 |
Dielectric Constant, 1 MHz |
3.68 |
- |
JIS C 2138 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Optical properties | Value | Unit | Test Standard |
ISO Data |
Haze |
2 |
- |
ISO 14782 |
Other Standards[S] |
Light Transmittance |
93 |
% |
ISO 13468-1 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Density |
1120 |
kg/m³ |
ISO 1183 |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Pre-drying - Temperature |
70 - 80 |
°C |
- |
Pre-drying - Time |
4 |
h |
- |
Melt temperature |
200 - 230 |
°C |
- |
Mold temperature |
20 - 40 |
°C |
- |
Screw speed |
<100 |
rpm |
- |
Back pressure |
0 - 5 |
MPa |
- |
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
U.V. stabilized or stable to weather, Transparent
Features
Blending Resin, Low Odor, Copolymer
Chemical Resistance
Acid Resistance, Alkali Resistance, Oil Resistance
Applications
Automotive, Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com