Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEONA™ 1302S - PA66 - Asahi Kasei

Material Data Center offers the following functions for LEONA™ 1302S:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Leona datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 3000 / 1200 MPa ISO 527
Yield stress 82 / 52 MPa ISO 527
Yield strain 4 / 24 % ISO 527
Strain at break - / >50 % ISO 527
Flexural modulus, 23°C 2700 / 1100 MPa ISO 178
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6 / 15 kJ/m² ISO 179/1eA
Rockwell hardness R 120 - ISO 2039-2
ASTM Data
Tensile Strength 79 / 57 MPa ASTM D 638
Elongation at Break 50 / 250 % ASTM D 638
Flexural Modulus 8200 / 1200 MPa ASTM D 790
Flexural Strength 118 / 54 MPa ASTM D 790
Rockwell Hardness M 80 / - ASTM D 785
Taber Abrasion Resistance 7 mg/1000 cycles ASTM D 1044
Izod Impact notched, 1/8 in 39 / 147 J/m ASTM D 256
Thermal propertiesdry / condUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 70 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 190 / * °C ISO 75-1/-2
Burning behav. at thickness h V-2 / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
ASTM Data
UL 94 Flame rating V-2 - UL 94
Thickness tested 1.6 mm -
Coefficient of Thermal Expansion, MD 79.9 E-6/K ASTM D 696
DTUL @ 66 psi 230 °C ASTM D 648
DTUL @ 264 psi 70 °C ASTM D 648
Limiting Oxygen Index 26 % ASTM D 2863
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E12 / - Ohm*m IEC 62631-3-1
Electric strength 20 / - kV/mm IEC 60243-1
Comparative tracking index 575 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Humidity absorption 2.5 / * % Sim. to ISO 62
Density 1140 / - kg/m³ ISO 1183
Density 1140 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 2 - 3 h -
Melt temperature 270 - 290 °C -
Mold temperature 75 - 85 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Features
Color Stability
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.