Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY GP1000MR - PC - LG Chem

Material Data Center offers the following functions for LUPOY GP1000MR:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 11 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mold Shrinkage, MD 0.0065 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 61.8 MPa ASTM D 638
Elongation at Break 150 % ASTM D 638
Flexural Modulus 2256 MPa ASTM D 790
Flexural Strength 98.1 MPa ASTM D 790
Rockwell Hardness R 118 - ASTM D 785
Izod Impact notched, 1/8 in 707 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 1.5 mm -
DTUL @ 264 psi 130 °C ASTM D 648
Vicat Temperature 141 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ISO Data
Comparative tracking index 250 - IEC 60112
ASTM Data
Volume Resistivity 2E15 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 - 120 °C -
Pre-drying - Time 3 - 5 h -
Processing humidity ≤0.02 % -
Melt temperature 300 - 320 °C -
Mold temperature 80 - 120 °C -
Zone 1 260 - 280 °C -
Zone 2 280 - 300 °C -
Zone 3 300 - 320 °C -
Nozzle temperature 300 - 320 °C -
Screw speed 40 - 70 rpm -
Back pressure 1 - 4 MPa -
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
Transparent
Applications
Automotive, IT / Business Machine, Electrical and Electronical, General Purpose
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.