Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® ECO 358N BC70 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® ECO 358N BC70:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Luran® ECO 358N BC70 is the general purpose easy-flow grade of SAN, suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very good transparency and a light intrinsic color. Luran® ECO 358N BC70 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 93 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 70 %
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 22 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Molding shrinkage, parallel 0.5 % ISO 294-4, 2577
Thermal conductivity of melt 0.17 W/(m K) -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3700 MPa ISO 527
Stress at break 72 MPa ISO 527
Strain at break 3 % ISO 527
Flexural modulus, 23°C 3600 MPa ISO 178
Flexural strength 120 MPa ISO 178
Charpy impact strength, +23°C 16 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 16 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 2 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 2 kJ/m² ISO 180/1A
Ball indentation hardness 165 MPa ISO 2039-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 86 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 99 °C ISO 75-1/-2
Vicat softening temperature, B 106 °C ISO 306
Coeff. of linear therm. expansion, parallel 70 E-6/K ISO 11359-1/-2
Other Standards[S]
Thermal Conductivity, solid state 0.17 W/(m K) DIN 52612-1
S: These properties are reported by the producer according standards that are different to our defaults.
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3 - IEC 62631-2-1
Dissipation factor, 100Hz 40 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 70 E-4 IEC 62631-2-1
Volume resistivity 1E14 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Optical propertiesValueUnitTest Standard
Other Standards[S]
Index of Refraction 1.57 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesValueUnitTest Standard
Humidity absorption 0.2 % Sim. to ISO 62
Density 1080 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 220 - 260 °C -
Mold temperature 40 - 80 °C -
Injection speed 200 mm/s -
Diagrams
Viscosity-shear rate , Luran® ECO 358N BC70, SAN, INEOS Styrolution
Shearstress-shear rate , Luran® ECO 358N BC70, SAN, INEOS Styrolution
Stress-strain , Luran® ECO 358N BC70, SAN, INEOS Styrolution
Secant modulus-strain , Luran® ECO 358N BC70, SAN, INEOS Styrolution
Stress-strain (isochronous) 23°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep modulus-time 23°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep curve 23°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Stress-strain (isochronous) 40°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep modulus-time 40°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep curve 40°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Stress-strain (isochronous) 60°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep modulus-time 60°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep curve 60°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Stress-strain (isochronous) 80°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep modulus-time 80°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Creep curve 80°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
Specific volume-temperature (pvT) , Luran® ECO 358N BC70, SAN, INEOS Styrolution
Tensile modulus-temperature , Luran® ECO 358N BC70, SAN, INEOS Styrolution
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat, Transparent
Chemical Resistance
General Chemical Resistance
Certifications
Contains renewable resources, Food contact, ISCC Plus
Applications
General Purpose, Packaging
Regional Availability
North America, Europe, Asia Pacific, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 260°C

Mold temperature, range: 40 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com