Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® HH-120 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® HH-120:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Luran® HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high heat ABS and PVC.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 7 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Thermal conductivity of melt 0.17 W/(m K) -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3900 MPa ISO 527
Stress at break 79 MPa ISO 527
Strain at break 3 % ISO 527
Charpy impact strength, +23°C 20 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 21 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 2 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 104 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 110 °C ISO 75-1/-2
Vicat softening temperature, B 120 °C ISO 306
Coeff. of linear therm. expansion, parallel 70 E-6/K ISO 11359-1/-2
Other propertiesValueUnitTest Standard
Humidity absorption 0.3 % Sim. to ISO 62
Density 1080 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 220 - 270 °C -
Mold temperature 40 - 80 °C -
Diagrams
Viscosity-shear rate , Luran® HH-120, SAN, INEOS Styrolution
Shearstress-shear rate , Luran® HH-120, SAN, INEOS Styrolution
Stress-strain , Luran® HH-120, SAN, INEOS Styrolution
Secant modulus-strain , Luran® HH-120, SAN, INEOS Styrolution
Tensile modulus-temperature , Luran® HH-120, SAN, INEOS Styrolution
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets
Special Characteristics
Transparent
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 270°C

Mold temperature, range: 40 - 80°C

Other extrusion
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Prepreg, Melt temperature: 180 - 230°C

Pipes, Melt temperature: 180 - 230°C

Profile extrusion
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Profiles, Melt temperature: 230°C

Sheet extrusion
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Plates, Melt temperature: 180 - 230°C

Chemical Media Resistance
Acids
Nitric Acid (40% by mass) (23°C)
Alcohols
Isopropyl alcohol (23°C)
Hydrocarbons
n-Hexane (23°C)
Toluene (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Other
Ethyl Acetate (23°C)
Application examples
Corrugated sheet, roof, greenhouse
Door pillar, Skoda Superb
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.