Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S KR2950 - (ASA+PMMA) - INEOS Styrolution

Material Data Center offers the following functions for Luran® S KR2950:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Luran® S KR2950 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S KR2950 is an ASA/PMMA-blend providing brilliant colors, high surface gloss and enhanced scratch resistance..
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 10 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2100 MPa ISO 527
Yield stress 49 MPa ISO 527
Yield strain 3.6 % ISO 527
Charpy impact strength, +23°C 160 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 54 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 9 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 3 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 96 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 100 °C ISO 75-1/-2
Vicat softening temperature, A 91 °C ISO 306
Vicat softening temperature, B 91 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Other propertiesValueUnitTest Standard
Density 1100 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 240 - 280 °C -
Mold temperature 40 - 80 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
U.V. stabilized or stable to weather
Features
High Gloss, Scratch Resistant
Chemical Resistance
General Chemical Resistance
Regional Availability
Europe, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 240 - 280°C

Mold temperature, range: 40 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.