Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Promyde® B30 P2 HI60 - PA6 - Nurel S.A.

Material Data Center offers the following functions for Promyde® B30 P2 HI60:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Promyde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 120 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.8 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 2100 / 1300 MPa ISO 527
Tensile Strength 60 / 35 MPa ISO 527
Yield strain 4.5 / 35 % ISO 527
Strain at break 35 / >50 % ISO 527
Flexural modulus, 23°C 1700 / 900 MPa ISO 178
Flexural strength 70 / 35 MPa ISO 178
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 65 / 125 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 20 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 222 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 50 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 120 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 120 / * E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.5 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Comparative tracking index 600 / - - IEC 60112
Other Standards[S]
Relative permittivity, 1MHz 2.7 / 4 - IEC 60250
Dissipation factor, 1MHz 160 / 1000 E-4 IEC 60250
Volume resistivity 1E13 / 1E11 Ohm*m IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesdry / condUnitTest Standard
Water absorption 8.1 / * % Sim. to ISO 62
Humidity absorption 2.6 / * % Sim. to ISO 62
Density 1100 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 125 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature <80 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 250 - 270 °C -
Mold temperature 40 - 80 °C -
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com