Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TPE ProvaMed® 1060 - TPE - ACTEGA DS GmbH

Material Data Center offers the following functions for TPE ProvaMed® 1060:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, CAE Interfaces

Check here, which other Provamed datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 8 g/10min ISO 1133
Temperature 230 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Stress at 100% elongation 1.7 MPa ISO 527
Strain at break TPE >300 % ISO 527
Compression set at 23 °C, 24h 18 % ISO 815
Compression set at 70 °C, 24h 91 % ISO 815
ASTM Data
Shore A Hardness 60 - ASTM D 2240
Shore D Hardness 15 - ASTM D 2240
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 162 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min -40 °C ISO 11357-1/-2
Other propertiesValueUnitTest Standard
Density 890 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 20 - 60 °C -
Feed temperature 20 - 30 °C -
Zone 1 140 - 230 °C -
Nozzle temperature 190 - 230 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets
Special Characteristics
Transparent, Sterilizable, Ethylene Oxide (EtO) Sterilization, Steam sterilization, Gamma irradiation sterilization
Chemical Resistance
Oxidation Resistance, Radiation Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Application examples
Tremor Spoon Attachment
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.