Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AECV BLACK T8L - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AECV BLACK T8L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
ISO 16396 - PA12, KGHL, C16-010

Rilsamid® AECV BLACK T8L resin is a black colored polyamide 12. 
This grade is designed for cable coating.


Main applications:
  • Wire and cable sheathing

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. for any use above this limit, please refer to our technical services.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 12 / * cm³/10min ISO 1133
Temperature 235 / * °C -
Load 2.16 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1350 / 1100 MPa ISO 527
Yield stress 41 / 37 MPa ISO 527
Yield strain 5 / 10 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy notched impact strength, +23°C - / 8 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C - / 6 kJ/m² ISO 179/1eA
Puncture - maximum force, -30°C - / 5000 N ISO 6603-2
Puncture energy, -30°C - / 70 J ISO 6603-2
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 55 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 135 / * °C ISO 75-1/-2
Vicat softening temperature, B 138 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 80 / * E-6/K ISO 11359-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4 / - - IEC 62631-2-1
Relative permittivity, 1MHz 3 / - - IEC 62631-2-1
Dissipation factor, 100Hz 431 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 193 / - E-4 IEC 62631-2-1
Volume resistivity - / 2E6 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E11 Ohm IEC 62631-3-2
Electric strength - / 40 kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.6 / * % Sim. to ISO 62
Density 1010 / 1010 kg/m³ ISO 1183
Diagrams
Stress-strain , Rilsamid® AECV BLACK T8L (dry), PA12, ARKEMA
Secant modulus-strain , Rilsamid® AECV BLACK T8L (dry), PA12, ARKEMA
Characteristics
Processing
Injection Molding, Other Extrusion, Coating
Delivery form
Pellets, Black
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Other extrusion
Processing conditions:
- Typical melt temperature (Min / recommended / Max): 250°C / 260°C / 270°C
- Drying time and temperature (only necessary for bags opened more than two hours): 4 - 8 hours at 80°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.