Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TPX® MX004 - PMP - Mitsui Chemicals America, Inc.

Material Data Center offers the following functions for TPX® MX004:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other TPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 25 g/10min ASTM D 1238
Temperature 260 °C -
Load 5 kg -
Mold Shrinkage, MD 1.5 mm/mm ASTM D 955
Mold Shrinkage, TD 1.1 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 1303 MPa ASTM D 638
Tensile Strength 20 MPa ASTM D 638
Tensile Strength at Yield 25 MPa ASTM D 638
Elongation at Break 30 % ASTM D 638
Flexural Modulus 1772 MPa ASTM D 790
Flexural Strength 32 MPa ASTM D 790
Rockwell Hardness R75 - ASTM D 785
Izod Impact notched, 1/8 in 24 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
Coefficient of Thermal Expansion, MD 380 E-6/K ASTM D 696
DTUL @ 66 psi 100 °C ASTM D 648
Vicat Temperature 165 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ASTM Data
Volume Resistivity 1E16 Ohm*cm ASTM D 257
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 0.7 % ASTM D 1003
Light Transmittance 94 % ASTM D 1003
Index of Refraction 1.46 - ASTM D 542
Other propertiesValueUnitTest Standard
Density 833 kg/m³ ASTM D 792
Characteristics
Processing
Injection Molding, Fiber Extrusion, Film Extrusion, Other Extrusion, Blow Molding
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com