Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TENAC™-C CF454 - POM-CF20 - Asahi Kasei

Material Data Center offers the following functions for TENAC™-C CF454:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tenac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 3.3 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Melt flow index, MFI 4 g/10min ISO 1133
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 13000 MPa ISO 527
Stress at break 130 MPa ISO 527
Strain at break 1 % ISO 527
Flexural modulus, 23°C 12500 MPa ISO 178
Charpy notched impact strength, +23°C 5 kJ/m² ISO 179/1eA
ASTM Data
Tensile Strength 118 MPa ASTM D 638
Elongation at Break 5 % ASTM D 638
Flexural Modulus 12200 MPa ASTM D 790
Flexural Strength 185 MPa ASTM D 790
Rockwell Hardness M 104 - ASTM D 785
Izod Impact notched, 1/8 in 39 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 163 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 166 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 65 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
ASTM Data
UL 94 Flame rating HB - UL 94
Coefficient of Thermal Expansion, MD 40 E-6/K ASTM D 696
Coefficient of Thermal Expansion, TD 90 E-6/K ASTM D 696
DTUL @ 66 psi 166 °C ASTM D 648
DTUL @ 264 psi 163 °C ASTM D 648
Other propertiesValueUnitTest Standard
Density 1460 kg/m³ ISO 1183
Water Absorption, 24hr 0.2 % ASTM D 570
Density 1460 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 3 - 4 h -
Melt temperature 180 - 210 °C -
Mold temperature 60 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets
Special Characteristics
Increased electrical conductivity, Anti-static
Features
Copolymer
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com