Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4331 G6 HR - PBT-I-GF30 - BASF

Material Data Center offers the following functions for Ultradur® B 4331 G6 HR:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Injection-moulding grade containing 30% glass-fibres, for rigid,tough and dimensionally stable technical parts, used in applications with highest demands on hydrolysis resistance such es automotive connectors and housings for electronic units under the hood.
The black colored product Ultradur® B4331 G6 HR BK15045 has a LS coloration (Laser Sensitive) and can be marked with Nd:YAG lasers.
The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.

Abbreviated designation according to ISO 1043: PBT-I-GF30
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 6 cm³/10min ISO 1133
Temperature 250 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.4 % ISO 294-4, 2577
Molding shrinkage, normal 1.0 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 8300 MPa ISO 527
Stress at break 115 MPa ISO 527
Strain at break 3.5 % ISO 527
Charpy impact strength, +23°C 75 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 75 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 14 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 223 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 205 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 220 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 20 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 215 E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity 1E13 Ohm*m IEC 62631-3-1
Surface resistivity 1E15 Ohm IEC 62631-3-2
Electric strength 41 kV/mm IEC 60243-1
Comparative tracking index 500 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1490 kg/m³ ISO 1183
Material specific propertiesValueUnitTest Standard
ISO Data
Viscosity number 100 cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 120 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.04 % -
Melt temperature 250 - 280 °C -
Mold temperature 60 - 100 °C -
Diagrams
Viscosity-shear rate , Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Shearstress-shear rate , Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Stress-strain , Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Secant modulus-strain , Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Stress-strain (isochronous) 23°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep modulus-time 23°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep curve 23°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Stress-strain (isochronous) 40°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep modulus-time 40°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep curve 40°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Stress-strain (isochronous) 90°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep modulus-time 90°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep curve 90°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Stress-strain (isochronous) 120°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep modulus-time 120°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep curve 120°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Stress-strain (isochronous) 160°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep modulus-time 160°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Creep curve 160°C, Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Tensile modulus-temperature , Ultradur® B 4331 G6 HR, PBT-I-GF30, BASF
Characteristics
Processing
Injection Molding
Special Characteristics
High impact or impact modified
Chemical Resistance
Hydrolytically Stable
Applications
Automotive, Electrical and Electronical, Encapsulation
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 280 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 80 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.