Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2640 Z6 R01 AT - (POM+PUR) - BASF

Material Data Center offers the following functions for Ultraform® N2640 Z6 R01 AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.

Abbreviated designation according to ISO 1043-1: POM-HI
Designation according to ISO 29988-POM-K,,M-GNPR,2-1
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 4.5 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Molding shrinkage, parallel 1.5 % ISO 294-4, 2577
Molding shrinkage, normal 1.5 % ISO 294-4, 2577
Ejection temperature 105 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1500 MPa ISO 527
Yield stress 40 MPa ISO 527
Yield strain 15 % ISO 527
Nominal strain at break >50 % ISO 527
Tensile creep modulus, 1h 825 MPa ISO 899-1
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 18 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 9 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 165 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 70 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 130 °C ISO 75-1/-2
Vicat softening temperature, B 110 °C ISO 306
Coeff. of linear therm. expansion, parallel 140 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4.5 - IEC 62631-2-1
Relative permittivity, 1MHz 4.3 - IEC 62631-2-1
Dissipation factor, 100Hz 100 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 250 E-4 IEC 62631-2-1
Volume resistivity 1E11 Ohm*m IEC 62631-3-1
Surface resistivity 1E12 Ohm IEC 62631-3-2
Electric strength 36 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 1 % Sim. to ISO 62
Humidity absorption 0.3 % Sim. to ISO 62
Density 1340 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 200 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 °C -
Pre-drying - Time 3 h -
Processing humidity ≤0.2 % -
Melt temperature 190 - 215 °C -
Mold temperature 60 - 80 °C -
Diagrams
Viscosity-shear rate , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Shearstress-shear rate , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Dynamic Shear modulus-temperature , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Stress-strain , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Secant modulus-strain , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Stress-strain (isochronous) 23°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep modulus-time 23°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep curve 23°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Stress-strain (isochronous) 40°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep modulus-time 40°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep curve 40°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Stress-strain (isochronous) 60°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep modulus-time 60°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep curve 60°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Stress-strain (isochronous) 80°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep modulus-time 80°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep curve 80°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Stress-strain (isochronous) 100°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep modulus-time 100°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep curve 100°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Stress-strain (isochronous) 120°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep modulus-time 120°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Creep curve 120°C, Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Specific volume-temperature (pvT) , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Tensile modulus-temperature , Ultraform® N2640 Z6 R01 AT, (POM+PUR), BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Features
Copolymer
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 215 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com