Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse ABS Fusion+ - ABS - BASF

Material Data Center offers the following functions for Ultrafuse ABS Fusion+:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 10 cm³/10min ISO 1133
Temperature 250 °C -
Load 5 kg -
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 114 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 71 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 91 °C ISO 75-1/-2
Other propertiesValueUnitTest Standard
Density 1070 kg/m³ ISO 1183
3D DataValueUnitTest Standard
Other Standards[S]
Tensile modulus, flat 1380 MPa ISO 527
Tensile modulus, upright 1110 MPa ISO 527
Tensile strength, flat 29.5 MPa ISO 527
Tensile strength, upright 17.9 MPa ISO 527
Strain at break, flat 10.9 % ISO 527
Strain at break, upright 2.1 % ISO 527
Flexural modulus, flat 1410 MPa ISO 178
Flexural modulus, on-edge 1130 MPa ISO 178
Flexural modulus, upright 878 MPa ISO 178
Flexural strength, flat 48.3 MPa ISO 178
Flexural strength, on-edge 48.7 MPa ISO 178
Flexural strength, upright 23.1 MPa ISO 178
Charpy impact strength, +23°C, flat 71.9 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, on-edge 119 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, upright 6.9 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, flat 32 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, on-edge 41.9 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, upright 2.5 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, flat 73.1 kJ/m² ISO 180/1U
Izod impact strength, +23°C, on-edge 131 kJ/m² ISO 180/1U
Izod impact strength, +23°C, upright 6.6 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, flat 26.4 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, on-edge 38.4 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, upright 2.2 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament
Features
Low Warpage
Applications
Automotive
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com