Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PLA PRO1 - PLA - BASF

Material Data Center offers the following functions for Ultrafuse PLA PRO1:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 18.2 cm³/10min ISO 1133
Temperature 210 °C -
Load 2.16 kg -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 175 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 63 °C ISO 11357-1/-2
Other propertiesValueUnitTest Standard
Density 1250 kg/m³ ISO 1183
3D DataValueUnitTest Standard
Other Standards[S]
Tensile modulus, flat 3170 MPa ISO 527
Tensile modulus, upright 2930 MPa ISO 527
Tensile strength, flat 48 MPa ISO 527
Tensile strength, upright 21.8 MPa ISO 527
Strain at break, flat 21.9 % ISO 527
Strain at break, upright 0.9 % ISO 527
Flexural modulus, flat 2820 MPa ISO 178
Flexural modulus, on-edge 2340 MPa ISO 178
Flexural strength, flat 92.4 MPa ISO 178
Flexural strength, on-edge 99.1 MPa ISO 178
Charpy impact strength, +23°C, flat 20.4 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, on-edge 18.8 kJ/m² ISO 179/1eU
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament
Certifications
Contains renewable resources
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.