Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Utec® 3041 - (PE-UHMW) - Braskem

Material Data Center offers the following functions for Utec® 3041:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Utec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 17 MPa ISO 527
Stress at break 30 MPa ISO 527
Strain at break 400 % ISO 527
Charpy impact strength, +23°C 180 kJ/m² ISO 179/1eU
Shore D hardness 64 - ISO 7619-1
ASTM Data
Tensile Strength at Yield 17 MPa ASTM D 638
Tensile Strength at Break 30 MPa ASTM D 638
Elongation at Break 350 % ASTM D 638
Shore D Hardness 64 - ASTM D 2240
Izod Impact notched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, A 128 °C ISO 306
ASTM Data
Coefficient of Thermal Expansion, MD 150 E-6/K ASTM D 696
DTUL @ 66 psi 79 °C ASTM D 648
DTUL @ 264 psi 48 °C ASTM D 648
Melting Temperature 133 °C ASTM D 3418
Vicat Temperature 128 °C ASTM D 1525
Thermal Conductivity, solid state 0.0577 W/(m K) ASTM C 177
Electrical propertiesValueUnitTest Standard
ASTM Data
Dielectric Strength, Short Time 90 kV/mm ASTM D 149
Surface Resistivity 1E12 Ohm ASTM D 257
Volume Resistivity 1E14 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.01 % ASTM D 570
Density 925 kg/m³ ASTM D 792
Intrinsic Viscosity 14 dl/g -
Bulk Density 450 kg/m³ -
Characteristics
Processing
Compression Molding
Special Characteristics
High impact or impact modified
Features
Tribologic Grade
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.