Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 2000 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 2000 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Medium viscosity, unreinforced polyether ether ketone

VESTAKEEP® 2000 G is a medium viscosity, unreinforced polyether ether ketone for injection molding.

The semi-crystalline polymer features superior, thermal and chemical resistance. Parts made from VESTAKEEP® 2000 G are of low flammability.

VESTAKEEP® 2000 G can be processed on common injection molding machines for thermoplastics.

We recommend a melt temperature between 360°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 2000 G is supplied as granules in 25 kg boxes with moisture-proof polyethylene inliners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect values.

For information about processing VESTAKEEP® 2000 G, please follow the general recommendations in our brochure "VESTAKEEP® PEEK Processing Guidelines“.

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.INDUSTRIAL.VESTAKEEP.COM
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 70 cm³/10min ISO 1133
Temperature 380 °C -
Load 5 kg -
Molding shrinkage, parallel 1.1 % ISO 294-4, 2577
Molding shrinkage, normal 1.1 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3700 MPa ISO 527
Yield stress 100 MPa ISO 527
Yield strain 5 % ISO 527
Nominal strain at break 20 % ISO 527
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
Charpy notched impact strength, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 340 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 150 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 155 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 205 °C ISO 75-1/-2
Vicat softening temperature, B 310 °C ISO 306
Coeff. of linear therm. expansion, parallel 60 E-6/K ISO 11359-1/-2
Yellow Card available yes - -
Oxygen index 38 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 2.8 - IEC 62631-2-1
Relative permittivity, 1MHz 2.8 - IEC 62631-2-1
Dissipation factor, 1MHz 50 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity 1E15 Ohm IEC 62631-3-2
Electric strength 32.6 kV/mm IEC 60243-1
Comparative tracking index 200 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.5 % Sim. to ISO 62
Humidity absorption 0.12 % Sim. to ISO 62
Density 1300 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 380 °C ISO 294
Injection Molding, mold temperature 180 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 120 MPa ISO 294
Diagrams
Stress-strain (isochronous) 150°C, VESTAKEEP® 2000 G, PEEK, Evonik
Creep modulus-time 150°C, VESTAKEEP® 2000 G, PEEK, Evonik
Creep curve 150°C, VESTAKEEP® 2000 G, PEEK, Evonik
Tensile modulus-temperature , VESTAKEEP® 2000 G, PEEK, Evonik
Characteristics
Processing
Injection Molding, Film Extrusion, Other Extrusion
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com