Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® i4 PL - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® i4 PL:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Implantable grade polyether ether ketone plates for permanent implants 
VESTAKEEP® i4 PL are plates based on implantable grade VESTAKEEP® i4 G neat polyether ether ketone resin.
 
Proven Biocompatibility of VESTAKEEP® i-Grades

The extra high purity and extended quality measures make VESTAKEEP® i-Grade materials an excellent choice for permanent implants.

For VESTAKEEP® i4 PL, biocompatibility has been tested according to ISO 10993-1 recommendations for permanent tissue/bone contact and USP Class VI.

VESTAKEEP® i4 PL complies ASTM F2026 “Standard Specification for Polyetheretherketone (PEEK) Polymers for Surgical Implant Applications”.

A summary of biocompatibility test results is available upon request.
 
Biocompatibility tests available for i4 PL

 
Delivery of VESTAKEEP® i-Grades
VESTAKEEP® i4 PL plates have thickness of up to 60 mm, standard width of 500 mm and standard length of 1000 mm.

Custom lengths are also available

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 4000 MPa ISO 527
Yield stress 109 MPa ISO 527
Yield strain 4.8 % ISO 527
Nominal strain at break >50 % ISO 527
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 340 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 155 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 205 °C ISO 75-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 2.8 - IEC 62631-2-1
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Humidity absorption 0.12 % Sim. to ISO 62
Density 1300 kg/m³ ISO 1183
Characteristics
Delivery form
Semifinished product
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.