Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7167 - PA12 FR(30) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7167:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

High viscosity, self-extinguishing PA12 compound, free of halogen and phosphorus

VESTAMID® X7167 NC is a heat stabilized PA12 compound containing a non-migrating flame retardant, free of halogen and phosphorous.
 

VESTAMID® X7167 NC complies with the requirements of FAR 25.853 or ABD 0031. The absence of halogens and phosphorous makes VESTAMID® X7167 NC especially suitable for interior parts in aircrafts, railways and ships.
 

This resin can be used for extrusion as well as for injection molding. Due to the presence of flame retardant melt temperature should not exceed 260 °C. We recommend melt temperatures of 210 - 230 °C.
 

VESTAMID® X7167 NC is supplied as cylindrical pellets, ready for use, in moisture-proof bags.

The use of colorants may affect property values. 


Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.


For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 


The values presented are typical or average values, they do not constitute a specification.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 4.1 / * cm³/10min ISO 1133
Temperature 230 / * °C -
Load 2.16 / * kg -
Molding shrinkage, parallel 0.6 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.9 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1700 / 1440 MPa ISO 527
Yield stress 47 / 42 MPa ISO 527
Yield strain 5 / 13 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 7 / 9 kJ/m² ISO 179/1eA
Type of failure C / C - -
Charpy notched impact strength, -30°C 6 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 130 / * °C ISO 75-1/-2
Vicat softening temperature, B 150 / * °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. V-2 / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Oxygen index 26 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz - / 4.8 - IEC 62631-2-1
Relative permittivity, 1MHz 3.6 / 3.2 - IEC 62631-2-1
Dissipation factor, 100Hz - / 800 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 380 / 400 E-4 IEC 62631-2-1
Volume resistivity 1E12 / 2E12 Ohm*m IEC 62631-3-1
Electric strength 34 / 36 kV/mm IEC 60243-1
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.5 / * % Sim. to ISO 62
Humidity absorption 0.6 / * % Sim. to ISO 62
Density 1050 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 240 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Characteristics
Processing
Injection Molding, Profile Extrusion, Other Extrusion
Delivery form
Pellets, Natural Color
Additives
Lubricants
Special Characteristics
Flame retardant, Halogen-free, Phosphorus-free, Heat stabilized or stable to heat
Applications
Aircraft and Aerospace
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com