Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L1930 BK 9.7503 - PA12-GD30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L1930 BK 9.7503:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Glass fiber-reinforced, heat stabilized polyamide 12 compound

VESTAMID® L1930 BK 9.7503 is a heat stabilized, with 30% milled glass fiber-reinforced PA 12 compound suitable for injection molding.

Due to the reinforcement moldings from this compound exhibit a high strength and rigidity. Because PA 12 absorbs only little water, the parts have a good dimensional stability and almost unaffected mechanical properties at changing ambient humidity.

Due to the reinforcement the shrinking of moldings is decreased compared with unreinforced compounds. Using specialty short glass fibers for the reinforcement of VESTAMID® L1930 BK 9.7503 the difference between longitudinal and transverse shrinkage relating to the flow direction of the melt is significantly lower than with common glass fiber-reinforced products. Therefore especially low-warpage precision parts can be molded.

As a semi-crystalline material VESTAMID® L1930 BK 9.7503 feature an outstanding chemical resistance, e.g., against fuels, oils and fats.

VESTAMID® L1930 BK 9.7503 is supplied as cylindrical pellets in moisture-proof packaging.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 27 / * cm³/10min ISO 1133
Temperature 250 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.5 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.5 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 3800 / 2970 MPa ISO 527
Yield stress 65 / 58 MPa ISO 527
Yield strain 5 / 8 % ISO 527
Nominal strain at break 11 / 15 % ISO 527
Charpy impact strength, +23°C 75 / 82 kJ/m² ISO 179/1eU
Type of failure C / C - -
Charpy impact strength, -30°C 65 / 72 kJ/m² ISO 179/1eU
Type of failure C / C - -
Charpy notched impact strength, +23°C 7 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Charpy notched impact strength, -30°C 6 / 5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 177 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 44 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 130 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 170 / * °C ISO 75-1/-2
Vicat softening temperature, B 170 / * °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4.2 / 5.3 - IEC 62631-2-1
Relative permittivity, 1MHz 3.5 / 3.5 - IEC 62631-2-1
Dissipation factor, 100Hz 360 / 860 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 340 / 460 E-4 IEC 62631-2-1
Volume resistivity 1E13 / 1.5E12 Ohm*m IEC 62631-3-1
Electric strength 48 / 45 kV/mm IEC 60243-1
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Humidity absorption 0.5 / * % Sim. to ISO 62
Density 1240 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 250 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Special Characteristics
Heat stabilized or stable to heat
Features
Low Warpage
Chemical Resistance
General Chemical Resistance, Grease Resistance, Oil Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.