Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9012 T8 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9012 T8:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Heat stabilized and light resistant polyamide 12 compound

VESTAMID® LX9012 T8 has been especially developed for the extrusion and co-extrusion of ski upper and decorative films. Decoration on the bottom side of injection molded sports shoe soles is a further application field.

Films made of VESTAMID® LX9012 T8 feature high transparency, good screen and sublimation printing, outstanding scratch resistance, and excellent impact strength at low temperatures. The semi-crystalline compounds based on PA 12 absorb only low quantities of water.

Therefore, molded parts show excellent dimensional stability, constantly high impact strength, low coefficient of friction and good chemical resistance at changing ambient humidity.

VESTAMID® LX9012 T8 is supplied as cylindrical granules, ready for processing in moisture-proof packaging.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 22 / * cm³/10min ISO 1133
Temperature 220 / * °C -
Load 10 / * kg -
Molding shrinkage, parallel 1.3 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.3 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1100 / - MPa ISO 527
Yield stress 35 / - MPa ISO 527
Yield strain 5 / - % ISO 527
Nominal strain at break >50 / - % ISO 527
Charpy impact strength, +23°C N / - kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 13 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Charpy notched impact strength, -30°C 15 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Shore D hardness 71 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 176 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 39 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 45 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 120 / * °C ISO 75-1/-2
Vicat softening temperature, B 130 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 130 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.8 / - - IEC 62631-2-1
Relative permittivity, 1MHz 3 / - - IEC 62631-2-1
Dissipation factor, 100Hz 530 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 280 / - E-4 IEC 62631-2-1
Volume resistivity 1E12 / - Ohm*m IEC 62631-3-1
Other propertiesdry / condUnitTest Standard
Water absorption 1.5 / * % Sim. to ISO 62
Humidity absorption 0.8 / * % Sim. to ISO 62
Density 1010 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding, Film Extrusion
Delivery form
Pellets
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, Heat stabilized or stable to heat, Transparent
Features
Scratch Resistant, Tribologic Grade
Chemical Resistance
General Chemical Resistance
Applications
Sports Equipment
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.