Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vitane LFC 9350 - TPU - geba Kunststoffcompounds GmbH

Material Data Center offers the following functions for Vitane LFC 9350:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Vitane datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Strength 15.5 MPa ISO 37
Strain at break 130 % ISO 37
Shore D hardness 50 - ISO 7619-1
Other Standards[S]
Stress at 10% elongation 0.7 MPa DIN 53504
S: These properties are reported by the producer according standards that are different to our defaults.
Electrical propertiesValueUnitTest Standard
Other Standards[S]
Volume resistivity 2 Ohm*m IEC 60093
Surface resistivity 400 Ohm IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesValueUnitTest Standard
Density 1270 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 220 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature <80 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
Melt temperature 210 - 230 °C -
Mold temperature 40 - 80 °C -
Feed temperature 60 - 80 °C -
Zone 1 210 - 220 °C -
Zone 2 210 - 220 °C -
Zone 3 220 - 230 °C -
Nozzle temperature 220 - 230 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
Increased electrical conductivity
Chemical Resistance
Oil Resistance
Applications
Electrical and Electronical, Packaging
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.