Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 63A - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 63A:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Vydyne 63A is a medium-viscosity resin used for injection-molding and extrusion compounding. It is desirable to include this neat resin in a formulation in which the melt strength of the final product is critical for the application. Vydyne 63A exhibits good initial color and it has a moisture level below 0.1%. This product offers high strength, rigidity and toughness over a broad range of demanding applications. Resistance of Vydyne 63A to heat, oil and wear is typical of PA66 neat resins.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 1.9 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.9 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 3200 / 1700 MPa ISO 527
Yield stress 85 / 55 MPa ISO 527
Yield strain 5 / 20 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6 / 25 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 5 / 9 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 260 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 68 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 190 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 100 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 100 / * E-6/K ISO 11359-1/-2
Other propertiesdry / condUnitTest Standard
Humidity absorption 2.5 / * % Sim. to ISO 62
Density 1140 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding, Film Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets, Natural Color
Features
Melt Strength
Chemical Resistance
General Chemical Resistance, Solvent Resistance, Oil Resistance
Applications
Automotive, General Purpose, Monofilament, Packaging
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com