Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of XAREC® N WA 7030 - (PA66+PS-SY)-GF30 - Idemitsu Chemicals

Material Data Center offers the following functions for XAREC® N WA 7030:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Xarec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
Other Standards[S]
Molding shrinkage, parallel 0.3 % Producer Method
Molding shrinkage, normal 0.8 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 10000 MPa ISO 527
Stress at break 175 MPa ISO 527
Strain at break 2.6 % ISO 527
Flexural modulus, 23°C 9100 MPa ISO 178
Flexural strength 250 MPa ISO 178
Charpy impact strength, +23°C 68 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 11 kJ/m² ISO 179/1eA
Izod impact strength, +23°C 57 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C 11 kJ/m² ISO 180/1A
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 245 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 260 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 24 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 49 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Comparative tracking index 325 - IEC 60112
ASTM Data
Dielectric Strength, Short Time 18 kV/mm ASTM D 149
Arc Resistance 150 s ASTM D 495
Other Standards[S]
Relative permittivity, 1MHz 3.2 - IEC 60250
Dissipation factor, 1MHz 690 E-4 IEC 60250
Volume resistivity 6.7E13 Ohm*m IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesValueUnitTest Standard
Density 1320 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 3 - 5 h -
Melt temperature 280 - 310 °C -
Mold temperature 50 - 80 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Applications
Automotive, Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.