Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BorShape™ FX1001 - PE - Borealis A/S

Material Data Center offers the following functions for BorShape™ FX1001:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, CAE Interfaces

Check here, which other BorShape datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 0.9 g/10min ISO 1133
Temperatura 190 °C -
Carga 5 kg -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 127 °C ISO 11357-1/-3
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Brillo 7 - ASTM D 2457
Opacidad 80 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 931 kg/m³ ISO 1183
Propiedades mecánicas (Film)ValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción, paralelo 350 MPa ISO 527-3
Módulo de tracción, normal 450 MPa ISO 527-3
Alargamiento máximo, paralelo 450 % ISO 527-3
Alargamiento máximo, normal 700 % ISO 527-3
Caida de dardo A 480 g ISO 7765-1
Coeficiente dinámico de fricción 0.4 - ISO 8295
Tipo de extrusión soplado - -
Espesor de la muestra 0.04 mm -
Recomendación para procesamiento ExtrusiónValorUnidadesMétodo de ensayo
Temperatura de la masa 190 - 210 °C -
Características
Procesamiento y forma de entrega
Extrusión de película soplada, Extrusion del film
Resistencia quimica
Resistencia a la oxidación
Certifications
Contacto con alimentos
Applicaciones
Empacado
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.