Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PP-GF30-0501P10/13 - PP-GLF30 - Celanese

Material Data Center offers the following functions for CELSTRAN® PP-GF30-0501P10/13:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Material code according to ISO 1043-1: PP Heat stabilized polypropylene reinforced with 30 weight percent long glass fibers. Black. The fibers are chemically coupled to the polypropylene matrix. The impact properties are enhanced. The pellets are cylindrical and normally as well as the embedded fibers 11  mm long. Parts molded of CELSTRAN have outstanding mechanical properties such as high strength and stiffness combined with high heat deflection. The notched impact strength is increased at elevated and low temperatures due to the fiber skeleton built in the parts. The long fiber reinforcement reduces creep significantly. The very isotropic shrinkage in the molded parts minimizes the warpage. Complex parts can be manufactured with high reproducibility by injection molding. Application field: Functional/structural parts for automotive

Flammability at thickness h (1 mm)HB-
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 6200 MPa ISO 527
Resistencia a la tracción 100 MPa ISO 527
Alargamiento a rotura 2.5 % ISO 527
Resistencia al impacto Charpy, +23°C 70 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 80 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 30 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 29 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 158 °C ISO 75-1/-2
Estabilidad al calor, 8.00 MPa 122 °C ISO 75-1/-2
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 1.0 mm -
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1120 kg/m³ ISO 1183
Funciones
Esfuerzo-alargamiento , CELSTRAN® PP-GF30-0501P10/13, PP-GLF30, Celanese
Módulo secante-alargamiento , CELSTRAN® PP-GF30-0501P10/13, PP-GLF30, Celanese
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro
Características especiales
Alto impacto o modificado al impacto, Estable contra el calor
Características
Refuerzo quimicamente acoplado, Resistencia a la fluencia, Long fiber reinforced, Baja deformación
Applicaciones
Automotriz
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.