Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Clearflex® H&T CLH 156 - (PE-LLD) - Versalis S.p.A

Material Data Center offers the following functions for Clearflex® H&T CLH 156:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Clearflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 2.5 g/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 120 °C ISO 11357-1/-3
Temp. reblandecimiento Vicat, A 95 °C ISO 306
Propiedades opticasValorUnidadesMétodo de ensayo
ISO Data
Brillo, 45° 91 - ISO 2813
Niebla 1 - ISO 14782
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 919 kg/m³ ISO 1183
Propiedades mecánicas (Film)ValorUnidadesMétodo de ensayo
ISO Data
Tensión a fluencia, paralelo 10 MPa ISO 527-3
Tensión a fluencia, normal 10 MPa ISO 527-3
Resistencia a la tracción, paralelo 30 MPa ISO 527-3
Resistencia a la tracción, normal 25 MPa ISO 527-3
Alargamiento máximo, paralelo 400 % ISO 527-3
Alargamiento máximo, normal 600 % ISO 527-3
Coeficiente dinámico de fricción 0.5 - ISO 8295
Tipo de extrusión colada - -
Espesor de la muestra 0.023 mm -
Características
Procesamiento y forma de entrega
Extrusion del film
Forma de suministro
Sémola
Características
Bajo gel
Resistencia quimica
Resistencia a la oxidación
Disponibilidad regional
Europa, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.