Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ Renew 401-50 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ Renew 401-50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastman Cristal™ Renew 401-50 copolyester is a high flow product that contains mold release for ease of ejection.

It is designed and engineered specifically for cosmetics packaging applications. With its unsurpassed color and

clarity and an unmatched ability to mold thick parts with improved gate aesthetics, Cristal 401-50 Renew is clearly

a well-suited copolyester for premium cosmetics packaging. Other outstanding features of Cristal™ Renew 401-50

copolyester are excellent chemical resistance, high gloss, and improvements in processing such as faster cycle

times, and lower scrap rates. Cristal Renew 401-50 is also ideally suited for two-shot molding techniques due to

its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a

global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are

produced with ISCC certified circular content by mass balance allocation.


Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.0035 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2030 MPa ISO 527
Esfuerzo de fluencia 50 MPa ISO 527
Alarg. en límite elástico 4.3 % ISO 527
Resistencia a la tracción 20 MPa ISO 527
Alargamiento a rotura 39 % ISO 527
ASTM Data
Módulo de tracción 2036 MPa ASTM D 638
Esfuerzo de fluencia a tracción 50 MPa ASTM D 638
Esfuerzo de fractura a tracción 24 MPa ASTM D 638
Alargamiento a la fluencia 4.4 % ASTM D 638
Alargamiento a la rotura 44 % ASTM D 638
Módulo de flexión 1808 MPa ASTM D 790
Resistencia a la flexión 66 MPa ASTM D 790
Dureza Rockwell R 108 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 103 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 44 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 68 °C ASTM D 648
Estabilidad al calor @ 264 psi 61 °C ASTM D 648
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 0.4 % ASTM D 1003
Transmitancia luminosa 91.8 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1280 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 65 °C -
Tiempo de pre-secado 8 h -
Temperatura de la masa 205 - 240 °C -
Temperatura del molde 16 - 38 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Forma de suministro
Color natural
Aditivos
Desmoldeante
Características especiales
Alto impacto o modificado al impacto, Transparente
Características
High Gloss, Copolímero
Resistencia quimica
Resistencia química general
Certifications
ISCC Plus
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.