Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CYCOLOY™ FR Resin CX7240 - Europe - (PC+ABS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for CYCOLOY™ FR Resin CX7240 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Cycoloy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
CYCOLOY CX7240 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, medium flow, non chlorinated/brominated flame retardant grade. It has a UL94 V0@.75mm, 5VA@3.0mm and 5VB@1.5mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications.

UL Yellow Card Link E45329-549531
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 15 cm³/10min ISO 1133
Temperatura 260 °C -
Carga 2.16 kg -
Densidad de fusión 1060 kg/m³ -
Conductibilidad termica de fusión 0.24 W/(m K) -
Calor especifico de la masa 2050 J/(kg K) -
Temperatura de expulsión 94 °C -
ASTM Data
Índice de fluidez, MFI 18 g/10min ASTM D 1238
Temperatura 260 °C -
Carga 2.16 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2600 MPa ISO 527
Esfuerzo de fluencia 65 MPa ISO 527
Alarg. en límite elástico 4 % ISO 527
Resistencia a la tracción 50 MPa ISO 527
Alargamiento a rotura 50 % ISO 527
Modulo de Flexión 2500 MPa ISO 178
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 22 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 10 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm N kJ/m² ISO 180/1U
Res. impacto Izod c/entalla, +23°C, 4mm 25 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 4mm 10 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 2600 MPa ASTM D 638
Esfuerzo de fluencia a tracción 65 MPa ASTM D 638
Esfuerzo de fractura a tracción 58 MPa ASTM D 638
Alargamiento a la fluencia 4.1 % ASTM D 638
Alargamiento a la rotura 100 % ASTM D 638
Módulo de flexión 2500 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 700 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 175 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 93 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 110 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 113 °C ISO 306
Coef.de expansión térmica lineal, paralelo 77 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 77 E-6/K ISO 11359-1/-2
Combustibilidad a espesor h V-2 class IEC 60695-11-10
Espesores de probeta 0.4 mm -
Combustibilidad 5V a espesor h 5VB class IEC 60695-11-20
Espesores de probeta 1.5 mm -
Conductibilidad termica 0.2 W/(m K) DIN 52616
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Estabilidad al calor @ 66 psi 100 °C ASTM D 648
Estabilidad al calor @ 264 psi 89 °C ASTM D 648
Temperatura Vicat 110 °C ASTM D 1525
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 35 kV/mm IEC 60243-1
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.2 % Sim. to ISO 62
Absorción de humedad 0.1 % Sim. to ISO 62
Densidad 1200 kg/m³ ISO 1183
Densidad 1190 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 - 90 °C -
Tiempo de pre-secado 2 - 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 250 - 300 °C -
Temperatura del molde 60 - 85 °C -
Temperatura - zona de alimentación 60 - 80 °C -
Zona 1 230 - 280 °C -
Zona 2 240 - 290 °C -
Zona 3 250 - 300 °C -
Funciones
Viscosidad-velocidad de cizallamiento , CYCOLOY™ FR Resin CX7240 - Europe, (PC+ABS), SABIC
Tensión de cizalla-velocidad de cizalla , CYCOLOY™ FR Resin CX7240 - Europe, (PC+ABS), SABIC
Volumen especifico-temperatura (pvT) , CYCOLOY™ FR Resin CX7240 - Europe, (PC+ABS), SABIC
Características
Procesamiento y forma de entrega
Moldeo por inyección
Aditivos
Ignifugante
Características especiales
Resistencia mejorada al fuego
Resistencia quimica
Resistencia química general
Applicaciones
Automotriz
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.