Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DOMAMID FR 6GT2010V0E - PA6-(GF+MD)20 - DOMO Engineering Plastics

Material Data Center offers the following functions for DOMAMID FR 6GT2010V0E:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Domamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 7900 / - MPa ISO 527
Resistencia a la tracción 85 / - MPa ISO 527
Alargamiento a rotura 3 / - % ISO 527
Módulo de flexión, 23°C 6500 / - MPa ISO 178
Resistencia a la flexión 120 / - MPa ISO 178
Resistencia al impacto Charpy, +23°C 35 / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 4.5 / - kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C 30 / - kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C 4.5 / - kJ/m² ISO 180/1A
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 221 / * °C ISO 11357-1/-3
Combustibilidad a 1.5mm esp. nom. V-0 / * class IEC 60695-11-10
Espesores de probeta 1.5 / * mm -
Combustibilidad a espesor h V-0 / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Ratio de combustión, FMVSS, espesor de 1mm 100 mm/min ISO 3795 (FMVSS 302)
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 2 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 1E13 / - Ohm*m IEC 62631-3-1
Resistividad superficial específica * / 1E13 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 575 / - - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1370 / - kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 75 - 85 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 240 - 260 °C -
Temperatura del molde 70 - 90 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características especiales
Resistencia mejorada al fuego, Sin halógeno, Sin fósforo
Características
Estabilidad térmica
Certifications
RoHS
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.