Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ A150 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ A150:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastar™ A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethanol. Eastar™ A150 is

intended primarily for extrusion into film and sheeting for packaging applications. It has excellent hydrolytic stability and good heat stability. Eastar™ A150 copolyester is lawful for use in food contact applications under food additive regulations published at 21 CFR 177.1240 by the Federal Food and Drug Administration. Therefore, it is lawful for use as a packaging material for meat or poultry foods prepared under federal inspection of the U.S. Department of Agriculture regulations at 9 CFR 318.7 and 381.147.




Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Temperatura de fusión 261 °C ASTM D 3418
Temperatura de transición vítrea 91 °C ASTM E 1356
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Brillo 108 - ASTM D 2457
Opacidad 0.5 % ASTM D 1003
Transmitancia luminosa 93 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ASTM D 792
Bulk Density 670 kg/m³ -
Propiedades mecánicas (Film)ValorUnidadesMétodo de ensayo
ASTM Data
Módulo de tracción, long. 1600 MPa ASTM D 882
Módulo de tracción, normal 1600 MPa ASTM D 882
Esfuerzo de fluencia a tracción, long. 43 MPa ASTM D 882
Esfuerzo de fluencia a tracción, normal 43 MPa ASTM D 882
Esfuerzo de fractura a tracción, long. 56 MPa ASTM D 882
Esfuerzo de fractura a tracción, normal 56 MPa ASTM D 882
Alargamiento a la fluencia, long. 5 % ASTM D 882
Alargamiento a la fluencia, normal 5 % ASTM D 882
Alargamiento a la rotura, long. 250 % ASTM D 882
Alargamiento a la rotura, normal 250 % ASTM D 882
Espesor de la muestra 0.28 mm -
Características
Procesamiento y forma de entrega
Extrusion del film, Extrusión de láminas
Características especiales
Estable contra el calor, Transparente
Características
Copolímero
Resistencia quimica
Estabilidad hidrolitica
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.