Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ BR003 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ BR003:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastar™ BR003 copolyester contains an additive that provides optimum molding efficiency. It has excellent appearance and is nearly water clear. With superior chemical resistance, it maintains its physical properties and appearance when exposed to aromatic oils. BR003 is specifically formulated to provide the optimal combination of chemical resistance, bristle retention, strength, stiffness, processability, clarity, colorability, and feel for toothbrushes. It also offers greater design flexibility and can work for virtually any toothbrush configuration; as a

result, brands can offer unique models that are tough to replicate—and launch them quicker. With BR003, molders can also consolidate resins versus having single resins for single designs. Under existing United States Food and Drug Administration(FDA) regulations, Eastar™ BR003 copolyester may lawfully be used to make food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240. Migration tests on BR003 samples meet the compliance requirements of 21 CFR 177.1240(e)(1),(2) and (3).




Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Módulo de flexión 2000 MPa ASTM D 790
Dureza Rockwell R 103 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 80 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 40 J/m ASTM D 256
Temperatura -40 °C -
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 0.3 % ASTM D 1003
Transmitancia luminosa 91 % ASTM D 1003
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 70 °C -
Tiempo de pre-secado 3 h -
Temperatura de la masa 230 - 280 °C -
Temperatura del molde 15 - 30 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Color natural
Características especiales
Transparente
Características
Copolímero
Resistencia quimica
Resistencia química general, Resistencia al aceite
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.