Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ MN005 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ MN005:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastar™ Copolyester MN005 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and EtO sterilization. Eastar™ Copolyester MN005 has excellent appearance and is nearly waterclear.


It is easy to process and can fill intricate tools. Its most outstanding features are exceptional clarity, toughness, radiation resistance chemical resistance and excellent color and property retention following gamma and e-beam sterilization. MN005 contains a mold release.




Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.003 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Esfuerzo de fluencia a tracción 47 MPa ASTM D 638
Esfuerzo de fractura a tracción 38 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 260 % ASTM D 638
Módulo de flexión 1900 MPa ASTM D 790
Dureza Rockwell 104 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in N J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 69 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 70 °C ASTM D 648
Estabilidad al calor @ 264 psi 67 °C ASTM D 648
Temperatura Vicat 84 °C ASTM D 1525
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1 % ASTM D 1003
Transmitancia luminosa 90 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua, 24hr 0.15 % ASTM D 570
Densidad 1230 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 75 °C -
Tiempo de pre-secado 6 h -
Temperatura de la masa 250 - 270 °C -
Temperatura del molde 15 - 30 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Aditivos
Desmoldeante
Características especiales
Transparente, Esterilizable, Esterilización por óxido de etileno (EtO), Gamma irradiation sterilization, Electron beam (e-beam) sterilization
Características
Estabilidad de color, Copolímero
Resistencia quimica
Resistencia química general, Resistencia a solventes, Resistencia a la radiacion
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR, Grado médico, Biocompatibility ISO 10993, USP Class VI
Applicaciones
Médico
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.