Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN001 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN001:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastar™ EN001 Copolyester is a thermoplastic polyester copolymer and is suitable for food packaging applications.

Eastar™ EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming processes and helps maintain good clarity when processing much thicker sheet. Eastar™ EN001 copolyester can also be used for injection molding applications. It is the preferred general-purpose crystallizable PET for thermoforming.

Eastar™ EN001 copolyester is regulated for use in food packaging applications in accordance with US FDA Regulation 21 CFR 177.1315. It is lawful for use under US Department of Agriculture Food Safety Inspection Service regulations as a packaging material for meat or poultry food products prepared under federal inspection.




Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2400 MPa ISO 527
Esfuerzo de fluencia 57 MPa ISO 527
Resistencia a la tracción 25 MPa ISO 527
Alargamiento a rotura 120 % ISO 527
Módulo de flexión, 23°C 2300 MPa ISO 178
Resistencia al impacto Izod, +23°C N kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C 4.5 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 3.1 kJ/m² ISO 180/1A
Temperatura -40 °C -
Perforación - energía, +23°C 15 J ISO 6603-2
Dureza Rockwell R 114 - ISO 2039-2
ASTM Data
Módulo de tracción 2400 MPa ASTM D 638
Esfuerzo de fluencia a tracción 58 MPa ASTM D 638
Esfuerzo de fractura a tracción 25 MPa ASTM D 638
Alargamiento a la rotura 120 % ASTM D 638
Módulo de flexión 2500 MPa ASTM D 790
Dureza Rockwell 112 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 40 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 27 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 65 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 69 °C ISO 75-1/-2
ASTM Data
Estabilidad al calor @ 66 psi 68.9 °C ASTM D 648
Estabilidad al calor @ 264 psi 65 °C ASTM D 648
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1 % ASTM D 1003
Transmitancia luminosa 84 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1330 kg/m³ ISO 1183
Densidad 1330 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión, Termoconformación
Características
Copolímero
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR
Applicaciones
Automotriz, Empacado, Equipos deportivos
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.