Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KELON A FR H2 CETG/300-V0 - PA66-(GF+MX) - LATI Industria Termoplastici S.p.A.

Material Data Center offers the following functions for KELON A FR H2 CETG/300-V0:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kelon A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 0.6 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.7 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 10000 MPa ISO 527
Resistencia a la tracción 80 MPa ISO 527
Alargamiento a rotura 1.6 % ISO 527
Resistencia al impacto Charpy, +23°C 20 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 2 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 220 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 240 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 235 °C ISO 306
Coef.de expansión térmica lineal, paralelo 30 E-6/K ISO 11359-1/-2
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
ASTM Data
Combustibilidad UL 94 V-0 - UL 94
Espesores de probeta 0.75 mm -
Índice de oxigeno límite 36 % ASTM D 2863
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Indice comparativo de linea de fuga 400 - IEC 60112
ASTM Data
Resistividad superficial 1E12 Ohm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1610 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 90 - 100 °C -
Tiempo de pre-secado 3 h -
Temperatura de la masa 270 - 290 °C -
Temperatura del molde 70 - 100 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Aditivos
Ignifugante
Características especiales
Estable contra el calor
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.