Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kocetal® K900 - POM - Kolon Industries

Material Data Center offers the following functions for Kocetal® K900:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kocetal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 42 g/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 2.0 % ISO 294-4, 2577
ASTM Data
Índice de fluidez, MFI 42 g/10min ASTM D 1238
Temperatura 190 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.02 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de tracción 65 MPa ISO 527
Alargamiento a rotura 20 % ISO 527
Módulo de flexión, 23°C 2950 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 5 kJ/m² ISO 179/1eA
Dureza Rockwell M 82 - ISO 2039-2
ASTM Data
Esfuerzo de tracción 64 MPa ASTM D 638
Alargamiento a la rotura 45 % ASTM D 638
Módulo de flexión 2700 MPa ASTM D 790
Resistencia a la flexión 96 MPa ASTM D 790
Dureza Rockwell M 80 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 50 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 165 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 100 °C ISO 75-1/-2
ASTM Data
Combustibilidad UL 94 HB - UL 94
Espesores de probeta 0.8 mm -
Coeficiente de dilatación térmica, long. 130 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 158 °C ASTM D 648
Estabilidad al calor @ 264 psi 110 °C ASTM D 648
Temperatura de fusión 166 °C ASTM D 3418
Temperatura Vicat 162 °C ASTM D 1525
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 1E12 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 19 kV/mm IEC 60243-1
ASTM Data
Resistencia dieléctrica, tiempo corto 19 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 1 MHz 0.006 - ASTM D 150
Constante dieléctrica, 1 MHz 3.7 - ASTM D 150
Resistividad superficial >1E15 Ohm ASTM D 257
Resistividad volumétrica 1E14 Ohm*cm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1410 kg/m³ ISO 1183
Absorción de agua, 24hr 0.22 % ASTM D 570
Densidad 1410 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 - 90 °C -
Tiempo de pre-secado 3 h -
Temperatura de la masa ≤220 °C -
Temperatura del molde 60 - 80 °C -
Zona 1 180 °C -
Zona 2 190 °C -
Zona 3 190 °C -
Temperatura de boquilla 200 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Disponibilidad regional
Norteamérica, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.