Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KDE1010 - PA66 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KDE1010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.0215 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.0245 mm/mm ASTM D 955
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2300 / 950 MPa ISO 527
Esfuerzo de tracción 64 / 47 MPa ISO 527
Resistencia a la flexión 82 / 30 MPa ISO 178
Resistencia al impacto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 21 / 50 kJ/m² ISO 179/1eA
Dureza Rockwell R 112 - ISO 2039-2
ASTM Data
Módulo de tracción 2300 / 950 MPa ASTM D 638
Esfuerzo de tracción 64 / 47 MPa ASTM D 638
Módulo de flexión 2100 / 800 MPa ASTM D 790
Resistencia a la flexión 82 / 30 MPa ASTM D 790
Dureza Rockwell R 112 / - ASTM D 785
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 260 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 70 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 230 / * °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 70 / * E-6/K ISO 11359-1/-2
Combustibilidad a espesor h HB / * class IEC 60695-11-10
ASTM Data
Combustibilidad UL 94 HB - UL 94
Coeficiente de dilatación térmica, long. 70 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 230 °C ASTM D 648
Estabilidad al calor @ 264 psi 70 °C ASTM D 648
Temperatura de fusión 260 °C ASTM D 3418
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 3 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 0.02 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E14 / - Ohm*m IEC 62631-3-1
Resistencia dieléctrica 32 / - kV/mm IEC 60243-1
ASTM Data
Resistencia dieléctrica, tiempo corto 32 / - kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 1 MHz 0.02 / - - ASTM D 150
Constante dieléctrica, 1 MHz 3 / - - ASTM D 150
Resistividad volumétrica 1E14 / - Ohm*cm ASTM D 257
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1090 / - kg/m³ ISO 1183
Absorción de agua, 24hr 1.3 % ASTM D 570
Densidad 1090 kg/m³ ASTM D 792
Características
Características especiales
Alto impacto o modificado al impacto
Applicaciones
Automotriz
Disponibilidad regional
Norteamérica, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.