Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY PC 1300-30 - PC - LG Chem

Material Data Center offers the following functions for LUPOY PC 1300-30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Índice de fluidez, MFI 30 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.006 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Módulo de tracción 2340 MPa ASTM D 638
Esfuerzo de fluencia a tracción 60 MPa ASTM D 638
Esfuerzo de fractura a tracción 61 MPa ASTM D 638
Alargamiento a la fluencia 6 % ASTM D 638
Alargamiento a la rotura 150 % ASTM D 638
Módulo de flexión 2410 MPa ASTM D 790
Resistencia a la flexión 96 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 700 J/m ASTM D 256
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Combustibilidad a 1.5mm esp. nom. V-2 class IEC 60695-11-10
Espesores de probeta 1.6 mm -
Yellow Card disponible - -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 2 mm -
ASTM Data
Combustibilidad UL 94 V-2 - UL 94
Espesores de probeta 0.5 mm -
Coeficiente de dilatación térmica, long. 68 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 139[ann.] °C ASTM D 648
Estabilidad al calor @ 264 psi 122 °C ASTM D 648
Temperatura Vicat 144 °C ASTM D 1525
Índice de oxigeno límite 26 % ASTM D 2863
ann.: annealed
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Indice comparativo de linea de fuga 250 - IEC 60112
ASTM Data
Resistencia dieléctrica, tiempo corto 17 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 60 Hz 0.001 - ASTM D 150
Constante dieléctrica, 60 Hz 3 - ASTM D 150
Resistividad volumétrica 2E17 Ohm*cm ASTM D 257
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1.1 % ASTM D 1003
Transmitancia luminosa 89 % ASTM D 1003
Índice de refracción 1.59 - ASTM D 542
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua, 24hr 0.15 % ASTM D 570
Absorción de agua, equilibrio 0.32 % ASTM D 570
Densidad 1200 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Características especiales
Alto impacto o modificado al impacto, Estable contra el calor, Transparente
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com