Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® ECO 378P BC60 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® ECO 378P BC60:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Luran® ECO 378P is an easy flow grade of SAN with enhanced chemical resistance and mechanical strength. Luran® ECO 378P BC60 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 78 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 60 %
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 20 cm³/10min ISO 1133
Temperatura 220 °C -
Carga 10 kg -
Contracción posterior al moldeo, paralelo 0.5 % ISO 294-4, 2577
Conductibilidad termica de fusión 0.17 W/(m K) -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3800 MPa ISO 527
Resistencia a la tracción 75 MPa ISO 527
Alargamiento a rotura 3.5 % ISO 527
Módulo de flexión, 23°C 3730 MPa ISO 178
Resistencia a la flexión 135 MPa ISO 178
Resistencia al impacto Charpy, +23°C 19 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 19 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 2 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 2 kJ/m² ISO 180/1A
Ball indentation hardness 175 MPa ISO 2039-1
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 89 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 101 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 107 °C ISO 306
Coef.de expansión térmica lineal, paralelo 70 E-6/K ISO 11359-1/-2
Other Standards[S]
Conductividad térmica, estado sólido 0.17 W/(m K) DIN 52612-1
S: These properties are reported by the producer according standards that are different to our defaults.
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1 % ASTM D 1003
Transmitancia luminosa 89 % ASTM D 1003
Other Standards[S]
Índice de refracción 1.56 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de humedad 0.3 % Sim. to ISO 62
Densidad 1080 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 220 - 260 °C -
Temperatura del molde 40 - 80 °C -
Velocidad de inyección 200 mm/s -
Funciones
Viscosidad-velocidad de cizallamiento , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Tensión de cizalla-velocidad de cizalla , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Módulo de cizallamiento dinámico-temperatura , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Esfuerzo-alargamiento , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Módulo secante-alargamiento , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 23°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Módulo de plastodeformación-tiempo 23°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Curva de creep 23°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 40°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Módulo de plastodeformación-tiempo 40°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Curva de creep 40°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 60°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Módulo de plastodeformación-tiempo 60°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Curva de creep 60°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 80°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Módulo de plastodeformación-tiempo 80°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Curva de creep 80°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Volumen especifico-temperatura (pvT) , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Módulo a tensión-temperatura , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características especiales
Estable contra el calor, Transparente
Resistencia quimica
Resistencia química general
Certifications
Contiene recursos renovables, Contacto con alimentos, ISCC Plus
Applicaciones
Electrica
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, Próximo Oriente/Africa
Demás información
Moldeo por inyección
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 260°C

Mold temperature, range: 40 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.