Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® 378P G7 - SAN-GF35 - INEOS Styrolution

Material Data Center offers the following functions for Luran® 378P G7:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Luran® 378P G7 is a glass fiber-reinforced grade (35% GF) of SAN with very high stiffness and low thermal coefficient of linear expansion. It features good chemical and weathering resistance and is suitable for extrusion and injection molding.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 4 cm³/10min ISO 1133
Temperatura 220 °C -
Carga 10 kg -
Conductibilidad termica de fusión 0.21 W/(m K) -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 12000 MPa ISO 527
Resistencia a la tracción 110 MPa ISO 527
Alargamiento a rotura 2 % ISO 527
Resistencia al impacto Charpy, +23°C 17 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 17 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 4 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 104 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 108 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 109 °C ISO 306
Coef.de expansión térmica lineal, paralelo 25 E-6/K ISO 11359-1/-2
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de humedad 0.25 % Sim. to ISO 62
Densidad 1360 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 220 - 260 °C -
Temperatura del molde 60 - 80 °C -
Funciones
Viscosidad-velocidad de cizallamiento , Luran® 378P G7, SAN-GF35, INEOS Styrolution
Tensión de cizalla-velocidad de cizalla , Luran® 378P G7, SAN-GF35, INEOS Styrolution
Módulo de cizallamiento dinámico-temperatura , Luran® 378P G7, SAN-GF35, INEOS Styrolution
Esfuerzo-alargamiento , Luran® 378P G7, SAN-GF35, INEOS Styrolution
Módulo secante-alargamiento , Luran® 378P G7, SAN-GF35, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 23°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Módulo de plastodeformación-tiempo 23°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Curva de creep 23°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 40°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Módulo de plastodeformación-tiempo 40°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Curva de creep 40°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 60°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Módulo de plastodeformación-tiempo 60°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Curva de creep 60°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 80°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Módulo de plastodeformación-tiempo 80°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Curva de creep 80°C, Luran® 378P G7, SAN-GF35, INEOS Styrolution
Volumen especifico-temperatura (pvT) , Luran® 378P G7, SAN-GF35, INEOS Styrolution
Módulo a tensión-temperatura , Luran® 378P G7, SAN-GF35, INEOS Styrolution
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de perfiles, Otros tipos de extrusión
Forma de suministro
Sémola
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Demás información
Moldeo por inyección
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 260°C

Mold temperature, range: 40 - 80°C

Otros tipos de extrusión
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Prepreg, Melt temperature: 220 - 240°C

Pipes, Melt temperature: 220 - 240°C

Extrusión de perfiles
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Profiles, Melt temperature: 240°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.