Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S 757R - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S 757R:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Luran® S 757R acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S 757R is a general purpose ASA injection molding grade providing enhanced stiffness.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 8 cm³/10min ISO 1133
Temperatura 220 °C -
Carga 10 kg -
Densidad de fusión 960 kg/m³ -
Conductibilidad termica de fusión 0.17 W/(m K) -
Calor especifico de la masa 2210 J/(kg K) -
Temperatura de expulsión 95 °C -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2600 MPa ISO 527
Esfuerzo de fluencia 56 MPa ISO 527
Alarg. en límite elástico 3.1 % ISO 527
Alarg. nominal a rotura 8 % ISO 527
Resistencia al impacto Charpy, +23°C 160 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 12 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 3 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 97 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 101 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 98 °C ISO 306
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 3.0 mm -
Yellow Card disponible - -
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 1.65 % Sim. to ISO 62
Absorción de humedad 0.35 % Sim. to ISO 62
Densidad 1070 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 240 - 280 °C -
Temperatura del molde 40 - 80 °C -
Funciones
Viscosidad-velocidad de cizallamiento , Luran® S 757R, ASA, INEOS Styrolution
Tensión de cizalla-velocidad de cizalla , Luran® S 757R, ASA, INEOS Styrolution
Esfuerzo-alargamiento , Luran® S 757R, ASA, INEOS Styrolution
Módulo secante-alargamiento , Luran® S 757R, ASA, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 23°C, Luran® S 757R, ASA, INEOS Styrolution
Módulo de plastodeformación-tiempo 23°C, Luran® S 757R, ASA, INEOS Styrolution
Curva de creep 23°C, Luran® S 757R, ASA, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 40°C, Luran® S 757R, ASA, INEOS Styrolution
Módulo de plastodeformación-tiempo 40°C, Luran® S 757R, ASA, INEOS Styrolution
Curva de creep 40°C, Luran® S 757R, ASA, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 60°C, Luran® S 757R, ASA, INEOS Styrolution
Módulo de plastodeformación-tiempo 60°C, Luran® S 757R, ASA, INEOS Styrolution
Curva de creep 60°C, Luran® S 757R, ASA, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 80°C, Luran® S 757R, ASA, INEOS Styrolution
Módulo de plastodeformación-tiempo 80°C, Luran® S 757R, ASA, INEOS Styrolution
Curva de creep 80°C, Luran® S 757R, ASA, INEOS Styrolution
Volumen especifico-temperatura (pvT) , Luran® S 757R, ASA, INEOS Styrolution
Módulo a tensión-temperatura , Luran® S 757R, ASA, INEOS Styrolution
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Desmoldeante
Características especiales
Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Disponibilidad regional
Europa, Asia Pacifico, Próximo Oriente/Africa
Demás información
Moldeo por inyección
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 240 - 280°C

Mold temperature, range: 40 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.