Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® ET3117 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® ET3117 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
  • MVR (300 °C/1.2 kg) 6.0 cm³/10 min
  • Extrusion
  • high viscosity
  • UV stabilized
  • solid sheet
  • corrugated sheet
Partially bio-circular grade / Attributed via mass balance (according to ISCC PLUS Standard).
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 6 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Índice de fluidez, MFI 6.5 g/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.7 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2350 MPa ISO 527
Esfuerzo de fluencia 65 MPa ISO 527
Alarg. en límite elástico 6.3 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Módulo de flexión, 23°C 2400 MPa ISO 178
Resistencia a la flexión 98 MPa ISO 178
Módulo de plastodeformación, 1h 2200 MPa ISO 899-1
Módulo de plastodeformación, 1000h 1900 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C, 3mm 80 kJ/m² ISO 179/1eA
Type of failure P - -
Resistencia al impacto Charpy c/entalla, -30°C, 3mm 14 kJ/m² ISO 179/1eA
Type of failure C - -
Resistencia al impacto Izod con entalla, +23°C 70 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 20 kJ/m² ISO 180/1A
Temperatura -30 °C -
Perforación - máxima fuerza, +23°C 5600 N ISO 6603-2
Perforación - máxima fuerza, -30°C 6500 N ISO 6603-2
Perforación - energía, +23°C 60 J ISO 6603-2
Perforación - energía, -30°C 70 J ISO 6603-2
Ball indentation hardness 112 MPa ISO 2039-1
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. de transición vítrea, 10°C/min 148 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 128 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 141 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 148 °C ISO 306
Coef.de expansión térmica lineal, paralelo 65 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 65 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad a espesor h V-2 class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Yellow Card disponible - -
Combustibilidad según índice de oxigeno 28 % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 875 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 875 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 900 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.1 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 8 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 100 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 34 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 250 - IEC 60112
Propiedades opticasValorUnidadesMétodo de ensayo
ISO Data
Niebla 0.8 - ISO 14782
Transmitancia luminosa 89 % ISO 13468-1, -2
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.3 % Sim. to ISO 62
Absorción de humedad 0.12 % Sim. to ISO 62
Densidad 1200 kg/m³ ISO 1183
Bulk density 660 kg/m³ -
Propiedades mecánicas (Film)ValorUnidadesMétodo de ensayo
ISO Data
WVTR, 23°C/85%r.h. 15 g/(m²*d) ISO 15106-1/-2
Espesor de la muestra 0.1 mm -
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 300 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de perfiles, Extrusión de láminas, Otros tipos de extrusión
Forma de suministro
Sémola
Aditivos
Desmoldeante
Características especiales
Estable contra rayos U.V./interperie
Certifications
Contiene recursos renovables, ISCC Plus
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.